when tig'n chromoly, what filler rod is used?
Thread Starter
Mr. Badwrench
Joined: May 2002
Posts: 14,146
Likes: 2
From: stranger in a strange land
<TABLE WIDTH="90%" CELLSPACING=0 CELLPADDING=0 ALIGN=CENTER><TR><TD>Quote, originally posted by tony1 »</TD></TR><TR><TD CLASS="quote">http://www.lincolnelectric.com...y.asp</TD></TR></TABLE>
thats a great link. i need to get off my *** and go to school for tig welding.
thats a great link. i need to get off my *** and go to school for tig welding.
most people will tell you to you an 80,000 psi tensile strength rod, like er80s-2. myself adn many others think a 70,000 rod is better for cromoly. the 80000 rod leaves too brittle of a weld and may crack over time. the 70000 rod will flex with the cromoly.